Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASFH16
Wavelength:
µm
(0.365 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.83294326-0.0156840611λ^{2}+0.0528843692λ^{-2}+0.00350978963λ^{-4}-0.000506491928λ^{-6}+0.000115081798λ^{-8}-1.10388704\text{×}10^{-05}λ^{-10}+5.01900181\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -4.41876e-07 1.0879e-08 1.5014e-12 1.0477e-06 1.44399e-09 0.264948 nd: 2.001000 Vd: 29.123651 density: 5.1 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.1e-06 K-1 dPgF: 0.0041 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links