Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASFH15
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.64640666-0.0151039558λ^{2}+0.0480157444λ^{-2}+0.00349072452λ^{-4}-0.000573639028λ^{-6}+0.000130249514λ^{-8}-1.29576789\text{×}10^{-05}λ^{-10}+5.92144355\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -5.7421e-07 1.1589e-08 -1.3886e-12 1.018e-06 1.3557e-09 0.26662 nd: 1.950000 Vd: 29.366344 density: 4.79 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.4e-06 K-1 dPgF: 0.005 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links