Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASF09
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.21640776-0.0137992658λ^{2}-0.000161434942λ^{4}+0.0281939284λ^{-2}+0.000509661263λ^{-4}+1.00848603\text{×}10^{-05}λ^{-6}+6.06649264\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.1218e-06 1.1539e-08 -1.0357e-12 7.1281e-07 8.2085e-10 0.15462 nd: 1.816000 Vd: 46.589656 glass_status: preferred density: 4.98 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.8e-06 K-1 dPgF: -0.0095 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links