Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASF014

Wavelength: µm
 (0.310–2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.1211948-0.0137527216λ^{2}-0.000186592469λ^{4}+0.0263764849λ^{-2}+0.00045369866λ^{-4}+1.09722341\text{×}10^{-05}λ^{-6}+6.11243363\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 23.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 2.5104e-06 1.1883e-08 -2.1145e-12 7.0672e-07 3.7726e-10 0.13495
nd: 1.788000
Vd: 47.354706
density: 4.36 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 5.7e-06 K-1
dPgF: -0.009
phosphate_resistance: 1.0

References

NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Hikari Glass Co., Ltd.

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.

External links


Glass

External links