Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASFH17
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.81220648-0.0171101271λ^{2}+0.0575348609λ^{-2}+0.00395166224λ^{-4}-0.000247712063λ^{-6}+3.77234212\text{×}10^{-05}λ^{-8}+0.000103512503λ^{4}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 2.000690 Vd: 25.454379 glass_status: preferred density: 4.68 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 dPgF: 0.0131
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon