Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF08
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.44097798-0.0140195736λ^{2}+0.0351597803λ^{-2}+0.000893152796λ^{-4}+2.96132309\text{×}10^{-06}λ^{-6}+1.83226713\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.882997 Vd: 40.764336 glass_code: 883408 glass_status: preferred density: 5.48 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 dPgF: -0.0092
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon