Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF04
Wavelength:
µm
(0.4 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.20360786-0.00877554777λ^{2}+0.0332446054λ^{-2}-0.000432887979λ^{-4}+0.000134715955λ^{-6}-4.716471\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.815540 Vd: 44.342093 glass_status: preferred density: 4.56 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.6e-06 K-1 dPgF: -0.009
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon