Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF02
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.15611691-0.0172799726λ^{2}+0.0273336859λ^{-2}+0.00119991815λ^{-4}-6.25674387\text{×}10^{-05}λ^{-6}+5.65571879\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.799520 Vd: 42.242361 glass_status: preferred density: 4.32 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 dPgF: -0.0075
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon