Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF016
Wavelength:
µm
(0.310 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.07241378-0.0146849804λ^{2}+0.0244285857λ^{-2}+0.000398183255λ^{-4}+1.22802438\text{×}10^{-05}λ^{-6}+1.23709929\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.772499 Vd: 49.607590 glass_code: 772496 glass_status: preferred density: 4.25 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.1e-06 K-1 dPgF: -0.009
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon