Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF014
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.12215038-0.0147958367λ^{2}+0.0260452483λ^{-2}+0.000507811768λ^{-4}+5.71446833\text{×}10^{-06}λ^{-6}+8.82357872\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.788001 Vd: 47.378774 glass_code: 788474 glass_status: preferred density: 4.36 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.1e-06 K-1 dPgF: -0.0089
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon