Optical constants of HIKARI - LaSF (Lanthanum dense flint)
E-LASF013
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.16454973-0.0146684282λ^{2}+0.030386787λ^{-2}+0.00102933823λ^{-4}-2.54435589\text{×}10^{-05}λ^{-6}+4.67271608\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.804398 Vd: 39.578982 glass_code: 804396 glass_status: preferred density: 4.2 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.5e-06 K-1 dPgF: -0.0052
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon