Optical constants of HIKARI - LaK (Lanthanum crown)
Q-LAK13S
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.82409056-0.0116215301λ^{2}-0.000136188911λ^{4}+0.0199712048λ^{-2}+0.000284067118λ^{-4}+7.76179707\text{×}10^{-06}λ^{-6}+6.22423374\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.4813e-06 1.5502e-08 -1.8528e-12 8.5107e-07 7.0734e-10 0.17132 nd: 1.697200 Vd: 53.288704 glass_status: preferred density: 3.74 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.1e-06 K-1 dPgF: -0.0067 phosphate_resistance: 4.0
Comments
For mold lens
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets