Optical constants of HIKARI - LaK (Lanthanum crown)
J-LAK9
Wavelength:
µm
(0.310 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.80700795-0.0135938061λ^{2}-0.000153406686λ^{4}+0.0188808096λ^{-2}+0.000280739188λ^{-4}+5.33547368\text{×}10^{-06}λ^{-6}+1.19947182\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.9877e-06 1.2157e-08 -1.5613e-12 5.0487e-07 6.0552e-10 0.17285 nd: 1.691000 Vd: 54.934151 glass_status: preferred density: 3.48 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.9e-06 K-1 dPgF: -0.0079 phosphate_resistance: 4.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon