Optical constants of HIKARI - LaK (Lanthanum crown)
J-LAK7R
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.68281356-0.012462194λ^{2}-0.000136478256λ^{4}+0.0162751692λ^{-2}+0.000253121787λ^{-4}+1.72812439\text{×}10^{-07}λ^{-6}+2.34124836\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.54376e-06 1.24315e-08 2.17432e-12 4.46388e-07 4.86384e-10 0.184172 nd: 1.651600 Vd: 58.618566 density: 3.34 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.1e-06 K-1 dPgF: -0.0051 phosphate_resistance: 4.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon