Optical constants of HIKARI - LaK (Lanthanum crown)
J-LAK18
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.93263885-0.0142564324λ^{2}-0.000192506617λ^{4}+0.0206017616λ^{-2}+0.000293008969λ^{-4}+6.61918495\text{×}10^{-06}λ^{-6}+7.33494598\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.411e-06 1.1591e-08 -1.5325e-12 5.5519e-07 3.2417e-10 0.13983 nd: 1.729160 Vd: 54.611531 density: 4.17 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.6e-06 K-1 dPgF: -0.0085 phosphate_resistance: 3.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links