Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK8
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.87864541-0.0142314931λ^{2}+0.0198025768λ^{-2}+0.00040117957λ^{-4}-6.68878586\text{×}10^{-06}λ^{-6}+7.86869747\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.712995 Vd: 53.875777 glass_code: 713539 glass_status: preferred density: 3.72 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 dPgF: -0.0081
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon