Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK7

Wavelength: µm
 (0.280 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.68241693-0.0118445415λ^{2}+0.016242269λ^{-2}+0.000303298585λ^{-4}-8.32486246\text{×}10^{-06}λ^{-6}+7.74390846\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 23.0 ℃
nd: 1.651597
Vd: 58.543058
glass_code: 652585
glass_status: preferred
density: 3.3 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8.1e-06 K-1
dPgF: -0.0039

References

NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Hikari Glass Co., Ltd.

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.

External links


Glass