Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK13
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.81365515-0.0134879998λ^{2}+0.0191920754λ^{-2}+0.000414986834λ^{-4}-7.45390097\text{×}10^{-06}λ^{-6}+7.65453719\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.693501 Vd: 53.203153 glass_code: 694532 glass_status: preferred density: 3.68 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.4e-06 K-1 dPgF: -0.0078
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon