Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK12
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.78094755-0.0236624998λ^{2}+0.00867653717λ^{-2}+0.00294181002λ^{-4}-0.000351554137λ^{-6}+1.84406503\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.677900 Vd: 55.397503 glass_status: preferred density: 3.96 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 dPgF: -0.007
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets