Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK10
Wavelength:
µm
(0.300 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.89528358-0.0117686807λ^{2}+0.0222295765λ^{-2}+0.000269351264λ^{-4}+2.23005932\text{×}10^{-05}λ^{-6}-4.3546434\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.719995 Vd: 50.228454 glass_code: 720502 glass_status: preferred density: 3.74 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.2e-06 K-1 dPgF: -0.0065
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)