Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK09
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.95310231-0.0196724731λ^{2}+0.0174257922λ^{-2}+0.00152866545λ^{-4}-0.000137028672λ^{-6}+6.72353302\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.734000 Vd: 51.483015 glass_code: 734515 glass_status: preferred density: 4.06 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.9e-06 K-1 dPgF: -0.0101
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)