Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK04
Wavelength:
µm
(0.4 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6768086-0.0102173269λ^{2}+0.0177389501λ^{-2}+2.82247162\text{×}10^{-05}λ^{-4}+4.32740016\text{×}10^{-05}λ^{-6}-2.15847266\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.651000 Vd: 56.171366 glass_status: preferred density: 3.26 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.1e-06 K-1 dPgF: -0.0012
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets