Optical constants of HIKARI - LaK (Lanthanum crown)
E-LAK02
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.74241958-0.0130203862λ^{2}+0.0159689321λ^{-2}+0.000709178831λ^{-4}-6.08192466\text{×}10^{-05}λ^{-6}+3.51166538\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.670000 Vd: 57.344444 glass_code: 670573 glass_status: preferred density: 3.74 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.8e-06 K-1 dPgF: -0.0045
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon