Optical constants of HIKARI - LaF (Lanthanum flint)
LAF9
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.097921-0.01112466λ^{2}+0.0388245λ^{-2}+0.001949184λ^{-4}-6.840198\text{×}10^{-05}λ^{-6}+1.330305\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.795040 Vd: 28.565137 glass_code: 795286 glass_status: preferred density: 4.97 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.5e-06 K-1 dPgF: 0.0036
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon