Optical constants of HIKARI - LaF (Lanthanum flint)
LAF7
Wavelength:
µm
(0.340 – 0.7)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.871638+0.05586319λ^{2}+0.08260113λ^{-2}-0.01257133λ^{-4}+0.00171414λ^{-6}-7.977217\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_is_absolute: false λ_is_vacuum: false temperature: 20.0 °C n_d: 1.749501 V_d: 35.186731 glass_code: 750352 glass_status: preferred density: 4.41 g/cm3 coefficient_of_thermal_expansion_1: 6.3e-06 K-1 ΔP_gF: -0.0027
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets