Optical constants of HIKARI - LaF (Lanthanum flint)
LAF3
Wavelength:
µm
(0.330 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.830874+0.02556412λ^{2}+0.05044859λ^{-2}-0.00670398λ^{-4}+0.0008789224λ^{-6}-4.052452\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.717000 Vd: 48.125992 glass_code: 717481 glass_status: preferred density: 3.77 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.9e-06 K-1 dPgF: -0.0078
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)