Optical constants of HIKARI - LaF (Lanthanum flint)
LAF11
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.809631+0.1142767λ^{2}+0.1251064λ^{-2}-0.0221709λ^{-4}+0.002916176λ^{-6}-0.0001356855λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.756920 Vd: 31.704801 glass_code: 757317 glass_status: preferred density: 4.58 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.4e-06 K-1 dPgF: -0.0001
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon