Optical constants of HIKARI - LaF (Lanthanum flint)
LAF09
Wavelength:
µm
(0.320 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.821152-0.012842λ^{2}+0.01957428λ^{-2}+0.0008519712λ^{-4}-3.820468\text{×}10^{-05}λ^{-6}+2.424251\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.697000 Vd: 48.530571 glass_code: 697485 glass_status: preferred density: 4.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.3e-06 K-1 dPgF: -0.0018
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon