Optical constants of HIKARI - LaF (Lanthanum flint)
J-LAF01
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.82684251-0.0103793494λ^{2}-7.59583803\text{×}10^{-05}λ^{4}+0.021662046λ^{-2}+0.000472548975λ^{-4}-2.58637501\text{×}10^{-06}λ^{-6}+1.43317138\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.9983e-07 1.0398e-08 -2.1837e-12 7.6422e-07 7.8937e-10 0.15326 nd: 1.700000 Vd: 48.103628 density: 3.68 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 dPgF: -0.0033 phosphate_resistance: 3.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets