Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF7
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.96631279-0.0109274208λ^{2}+0.0314277188λ^{-2}+0.000703288732λ^{-4}+4.43317688\text{×}10^{-05}λ^{-6}+2.65190331\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.749497 Vd: 35.281419 glass_code: 749353 glass_status: preferred density: 3.61 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.7e-06 K-1 dPgF: 0.0019
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets