Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF3
Wavelength:
µm
(0.4 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.88218387-0.0106317724λ^{2}+0.0227527853λ^{-2}+0.000397667212λ^{-4}+1.25478223\text{×}10^{-05}λ^{-6}+5.87511175\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.717004 Vd: 47.933096 glass_code: 717479 glass_status: preferred density: 3.89 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.6e-06 K-1 dPgF: -0.0033