Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF2
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9684827-0.0116032701λ^{2}+0.0244833672λ^{-2}+0.000775976856λ^{-4}-2.44342622\text{×}10^{-05}λ^{-6}+3.01832049\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.743997 Vd: 44.786312 glass_code: 744448 glass_status: preferred density: 4.16 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.6e-06 K-1 dPgF: -0.0037
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets