Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF05
Wavelength:
µm
(0.330 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.02046444-0.0121632364λ^{2}+0.028023846λ^{-2}+0.000861441681λ^{-4}-1.40486471\text{×}10^{-05}λ^{-6}+4.5613035\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.762001 Vd: 40.107044 glass_code: 762401 glass_status: preferred density: 3.94 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 dPgF: -0.0005
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon