Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF016
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.14158865-0.0147653343λ^{2}+0.0334231042λ^{-2}+0.00125430167λ^{-4}-3.49277287\text{×}10^{-05}λ^{-6}+8.7589435\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.800999 Vd: 34.963582 glass_code: 801350 glass_status: preferred density: 3.63 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.6e-06 K-1 dPgF: 0.0005
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon