Optical constants of HIKARI - LaF (Lanthanum flint)
E-LAF010
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.96201742-0.00690787335λ^{2}+0.0295340678λ^{-2}-0.00139338248λ^{-4}+0.000252317172λ^{-6}-1.245434\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.743200 Vd: 49.314451 glass_code: 743493 glass_status: preferred density: 4.07 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.6e-06 K-1 dPgF: -0.0089
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets