Optical constants of HIKARI - LLF (Very light flint)
LLF6
Wavelength:
µm
(0.300 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.326858-0.02496168λ^{2}+0.002979231λ^{-2}+0.003164392λ^{-4}-0.0003498773λ^{-6}+1.777229\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.531721 Vd: 49.142236 glass_code: 532491 glass_status: preferred density: 2.77 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.4e-06 K-1 dPgF: -0.0019
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon