Optical constants of HIKARI - LLF (Very light flint)
J-LLF2
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.32991556-0.00866190637λ^{2}-5.64810656\text{×}10^{-05}λ^{4}+0.01502038λ^{-2}+0.000420176461λ^{-4}-1.21206332\text{×}10^{-05}λ^{-6}+2.27699343\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -2.658e-06 8.2902e-09 -1.5376e-12 6.5839e-07 6.188e-10 0.23166 nd: 1.540720 Vd: 46.966429 density: 2.53 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.8e-06 K-1 dPgF: -0.0001 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets