Optical constants of HIKARI - LLF (Very light flint)
E-LLF6
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.30466-0.00864131348λ^{2}+0.0145944618λ^{-2}+0.000206597874λ^{-4}+1.88931616\text{×}10^{-05}λ^{-6}+1.82626789\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.531717 Vd: 48.862886 glass_code: 532489 glass_status: preferred density: 2.51 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.1e-06 K-1 dPgF: 0.0011
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon