Optical constants of HIKARI - LF (Light flint)
LF6
Wavelength:
µm
(0.310 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.402616-0.005310264λ^{2}+0.01706231λ^{-2}+0.000992587λ^{-4}-0.0001107158λ^{-6}+9.212954\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.567320 Vd: 42.699778 glass_code: 567427 glass_status: preferred density: 3.11 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.1e-05 K-1 dPgF: -0.002
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets