Optical constants of HIKARI - LF (Light flint)
LF5
Wavelength:
µm
(0.310 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.439252-0.005116676λ^{2}+0.02191912λ^{-2}-0.000308089λ^{-4}+0.0001181173λ^{-6}-4.409047\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.581440 Vd: 40.777871 glass_code: 581408 glass_status: preferred density: 3.24 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.06e-05 K-1 dPgF: -0.0008
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon