Optical constants of HIKARI - LF (Light flint)
E-LF6
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4026161-0.00531026402λ^{2}+0.0170623068λ^{-2}+0.000992586995λ^{-4}-0.000110715814λ^{-6}+9.21295404\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.567320 Vd: 42.699788 glass_status: preferred density: 2.54 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8e-06 K-1 dPgF: -0.002
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon