Optical constants of HIKARI - KzF (Special short flint)
KZFH2
Wavelength:
µm
(0.320 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.723491-0.01309285λ^{2}+0.02374514λ^{-2}+0.0007951295λ^{-4}-1.290725\text{×}10^{-05}λ^{-6}+3.339887\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.671629 Vd: 38.797887 glass_code: 672388 glass_status: preferred density: 1.0 g/cm3 dPgF: -0.0059
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon