Optical constants of HIKARI - KzF (Special short flint)
KZFH1
Wavelength:
µm
(0.310 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.547175-0.01287115λ^{2}+0.01838384λ^{-2}+0.0005862006λ^{-4}-1.624561\text{×}10^{-05}λ^{-6}+2.266107\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.612658 Vd: 44.404011 glass_code: 613444 glass_status: preferred density: 1.0 g/cm3 dPgF: -0.008
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon