Optical constants of HIKARI - KF (Crownflint)
J-KF6
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.26653222-0.00974283829λ^{2}-8.49115572\text{×}10^{-05}λ^{4}+0.0127195343λ^{-2}+0.000315395806λ^{-4}-8.83703038\text{×}10^{-06}λ^{-6}+1.84064027\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.0458e-06 1.7479e-08 -2.0062e-12 4.8402e-07 3.8942e-10 0.23771 nd: 1.517420 Vd: 52.203782 density: 2.47 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 dPgF: 0.0011 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets