Optical constants of HIKARI - K (Crown)
K5
Wavelength:
µm
(0.290 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.259379+0.009090504λ^{2}+0.02633942λ^{-2}-0.003777418λ^{-4}+0.0005228702λ^{-6}-2.629182\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.522490 Vd: 59.731237 glass_code: 522597 glass_status: preferred density: 2.61 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.02e-05 K-1 dPgF: 0.0026
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links