Optical constants of HIKARI - FK (Fluor crown)
P-FK01S
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2209843-0.00850617932λ^{2}+0.00565991749λ^{-2}+0.000843578948λ^{-4}-9.83647071\text{×}10^{-05}λ^{-6}+4.93916644\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.496488 Vd: 81.546118 glass_status: preferred density: 3.61 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.48e-05 K-1 dPgF: 0.0297
Comments
Low Tg glass
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links