Optical constants of HIKARI - FK (Fluor crown)
J-FKH2
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.10149795-0.00468337833λ^{2}-1.34642385\text{×}10^{-05}λ^{4}+0.00677542246λ^{-2}+4.53499889\text{×}10^{-05}λ^{-4}+2.24209054\text{×}10^{-06}λ^{-6}-6.21790903\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.9966e-05 -7.243e-09 -1.0192e-12 3.9302e-07 3.3541e-10 0.10384 nd: 1.456000 Vd: 91.374829 density: 3.67 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.34e-05 K-1 dPgF: 0.0431 phosphate_resistance: 4.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets