Optical constants of HIKARI - FK (Fluor crown)
J-FKH1
Wavelength:
µm
(0.280 – 2.400)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.22016073-0.00500725473λ^{2}-3.55507111\text{×}10^{-05}λ^{4}+0.00842088796λ^{-2}+7.02327459\text{×}10^{-05}λ^{-4}+2.470079\text{×}10^{-06}λ^{-6}-6.50002003\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.921e-05 -6.4099e-09 2.3373e-12 4.2686e-07 6.6656e-10 0.12235 nd: 1.497820 Vd: 82.571305 density: 3.86 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.29e-05 K-1 dPgF: 0.0327 phosphate_resistance: 4.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon