Optical constants of HIKARI - FK (Fluor crown)
E-FK5
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.1887621-0.0095572007λ^{2}+0.0089915232λ^{-2}+0.00014560516λ^{-4}-5.2843067\text{×}10^{-06}λ^{-6}+3.458801\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.487490 Vd: 70.406429 glass_code: 487704 glass_status: preferred density: 2.45 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.01e-05 K-1 dPgF: 0.0027
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon