Optical constants of HIKARI - F (Flint)
J-F3
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5354736-0.010429899λ^{2}-9.00763853\text{×}10^{-05}λ^{4}+0.0222719327λ^{-2}+0.000443442601λ^{-4}+7.40581279\text{×}10^{-05}λ^{-6}-6.90525545\text{×}10^{-06}λ^{-8}+6.52621989\text{×}10^{-07}λ^{-10}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.1828e-06 1.3656e-08 -1.4733e-12 7.3525e-07 9.8933e-10 0.2669 nd: 1.612930 Vd: 36.944974 glass_status: preferred density: 2.64 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.4e-06 K-1 dPgF: 0.004 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon